MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gromax 1163LL TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: 163LL is medium modulus grade with nominal Durometer hardness of 63D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and extrusion molding grade.

Characteristics:

  • Excellent low modulus for injection molding and extrusion molding grade.
  • Excellent flexibility and fatigue resistance.
  • Excellent creep resistance.
  • Excellent low shrinkage and higher melting temperature

    Information provided by Gromax Enterprises Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccISO 1183
Moisture Absorption 0.300 %
@Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.013 cm/cmISO 294-4
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63ISO 868
Tensile Strength 330 kg(f)/cm²ISO 527
Elongation at Break 487 %ISO 527
Tensile Modulus 511 MPaISO 527
Flexural Modulus 1830 kg(f)/cm²ISO 178
Charpy Impact, Notched NBISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.31e+13 ohm-cmIEC 60093
Surface Resistance 2.78e+15 ohmIEC 60093
Dielectric Strength 17.18 kV/mm
@Thickness 2.00 mm
IEC 60243-1
 
Thermal PropertiesOriginal ValueComments
Melting Point 212 °CISO 3146C
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 210 - 230 °C
Middle Barrel Temperature 230 - 260 °C
Front Barrel Temperature 230 - 260 °C
Nozzle Temperature 230 - 260 °C
Mold Temperature 20.0 - 50.0 °C
Injection Pressure 30.0 - 100 MPa
@Time 2.00 - 10.0 sec
Hold Pressure 5.00 - 40.0 MPa
@Time 10.0 - 30.0 sec
Screw Speed 40 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGROM051 / 147864

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.