MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC GELOY™ XP7550 ASA (Europe)
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: PC/ASA. Excellent weatherability.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D792
Density 1.11 g/ccISO 1183
Water Absorption 0.80 %23°C/sat; ISO 62
Moisture Absorption 0.300 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmSABIC method
 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 14 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 26 g/10 min
@Load 5.00 kg,
Temperature 260 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 109ASTM D785
Tensile Strength at Break 44.0 MPa50 mm/min; ISO 527
 44.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 55.0 MPa50 mm/min; ISO 527
 56.0 MPa50 mm/min; ASTM D638
Elongation at Break 37 %50 mm/min; ISO 527
 40 %50 mm/min; ASTM D638
Elongation at Yield 3.8 %50 mm/min; ISO 527
 4.0 %50 mm/min; ASTM D638
Tensile Modulus 2550 MPa1mm/min; ISO 527
 2550 MPa5 mm/min; ASTM D638
Flexural Yield Strength 74.0 MPa2 mm/min; ISO 178
 82.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2400 MPa2 mm/min; ISO 178
 2480 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 375 J/mASTM D256
 53.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 35.0 kJ/m²80*10*4; ISO 180/1A
 9.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 40.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 36.0 JASTM D3763
 10.0 J
@Temperature -30.0 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 72.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 72.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 78.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 79.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Hot Ball Pressure Test 85.0 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 103 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 104 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 89.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 89.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 105 °CRate B/50; ISO 306
 105 °CRate B/50; ASTM D1525
 106 °CRate B/120; ISO 306
 
Optical PropertiesOriginal ValueComments
Gloss 94 %60°; ASTM D523
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 240 - 255 °CInjection Molding
Zone 1 230 - 250 °C
Zone 2 240 - 255 °C
Zone 3 245 - 260 °C
Melt Temperature 255 - 270 °C
Mold Temperature 55.0 - 70.0 °C
Drying Temperature 90.0 - 100 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.040 %
Back Pressure 0.300 - 1.00 MPa
Shot Size 40 - 80 %
Vent Depth 0.00380 - 0.00760 cm
Screw Speed 30 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10156 / 243623

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.