MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik H10F Extra-fine Grain Cemented Carbide for Rotary Tools  (discontinued **)
Categories: Ceramic; Carbide; Metal; Metal Matrix Composite; Nonferrous Metal; Tungsten Alloy

Material Notes: SANDVIK extra-fine grain cemented carbide grades have been developed to meet the exacting demands placed on solid carbide tooling by modern technology.

SANDVIK extra-fine grain cemented carbide grades are true submicron grain size tungsten carbide alloys. The tungsten carbide grain size is 0.8 µm, which is precisely controlled.

This grade offers an excellent combination of strength and toughness. In addition, a special additive maximizes corrosion resistance without loss of toughness.

SANDVIK grade H10F incorporates 10% cobalt and 90% tungsten carbide (WC). H10F is recommended for solid carbide rotary tool applications in the ISO K20/K30 range. It has special advantages where high toughness and sharp edge profiles are needed.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 14.45 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell A 92.1
Hardness, Vickers 160030
Flexural Strength 4300 MPaTransverse Rupture; ISO 3327
Compressive Strength 6250 MPa
 
Component Elements PropertiesOriginal ValueComments
Cobalt, Co 10 %
WC 90 %
 
Descriptive Properties
Corrosion Resistance, 1-104
Wear Resistance, 0-105

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik H10F Cemented Carbide for Can Tooling
Sandvik H10F Cemented Carbide for Woodworking
Sandvik H11N Cemented Carbide for Metal Forming Applications
Kennametal Densalloy™ SD170
Sandvik H6F Cemented Carbide for Can Tooling

NSANDV033 / 18927

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.