MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Thermal Ceramics Superwool 607 HM 25 Bulk
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Superwool is designed from pure raw materials and specially processed to offer excellent performance in high temperature applications. Superwool offers an alternative to traditional solutions due to its exceptional properties of high refractoriness and excellent non-wetting characteristics in applications requiring direct contact with molten aluminum.

Superwool provides stability and resistance to chemical attack. Exceptions include hydrofluoric acid, phosphoric acid and strong alkalis (i.e. NaOH, KOH). Superwool is unaffected by incidental spills of oil or water. Thermal and physical properties are restored after drying.

Although Superwool’s basic fiber form offers an economical alternative for most applications, they can be engineered to meet the requirements of specific applications. Fiber diameter, shot content, fiber length and form can be altered as required to achieve desired properties for specific applications.

Features:

  • Low biopersistence
  • Thermal stability
  • Low heat storage
  • Good resistance to tearing
  • Flexible and resilient
  • Immune to thermal shock
  • Excellent thermal insulating performance
  • Based on patented technology
  • Applications

  • Expansion joints construction
  • Base seals
  • Low mass kiln car construction
  • Tube seal fabrication
  • Thermal and acoustical insulation
  • As primary raw material for high temperature converted and engineering fibers - Enfil®
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Bulk Density 0.192 - 0.256 g/cc
     
    Thermal PropertiesOriginal ValueComments
    Melting Point 2680 °F
    Maximum Service Temperature, Air 1832 °F
     
    Component Elements PropertiesOriginal ValueComments
    CaO 25 - 35 %
    MgO 4.0 - 7.0 %
    SiO2 60 - 70 %
     
    Descriptive Properties
    Alumina Contenttraces
    Fiber Length, cm<2.5

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    CTHERM276 / 2596

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.