MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Arlon 55572GA028 0.028" Cured Silicone Rubber with Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone, Molded, Glass Fiber Filled

Material Notes: Design/Construction:
  • Interleave: LDPE
  • Side 1: Cured Silicone Rubber
  • Substrate: Style 162 Fiberglass

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccSilicone Property; Arlon SQA-TMS-024
Thickness 12.0 milSide 1; Arlon SQA-TMS-003
 16.0 milSubstrate; Arlon SQA-TMS-003
 28.0 milOverall Thickness; Arlon SQA-TMS-003
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 44Silicone Property; Arlon SQA-TMS-014
Tensile Strength 1100 psiSilicone Property; Arlon SQA-TMS-008
Elongation at Break 650 %Silicone Property; Arlon SQA-TMS-008
Tear Strength 83.0 pliDie B; Silicone Property; Arlon SQA-TMS-029
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 457 V/milArlon SQA-TMS-020
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Inert 450 °F
Minimum Service Temperature, Air -70.0 °F
UL RTI, Electrical 428 °FE54153
UL RTI, Mechanical without Impact 392 °FE54153
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 204 °C
Recommended Post Cure Cycle
Shelf Life 60.0 Month
@Temperature 21.1 °C
 
Descriptive Properties
ColorGreen
Total Product Weight (oz/yd2)28.1Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PARL9795 / 148948

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.