MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Versify™ 3010 PE
Categories: Polymer; Thermoplastic

Material Notes: Product Description: Versity™ 3010 is a propylene ethylene copolymer with a medium melt flow rate manufactured with Dow’s Advanced Molecular Catalyst technology. It is suitable for cast film blown film and BOPP. It is an excellent sealant and is particularly suitable for use in BOPE structures. It has excellent compatibility with PP and is a useful agent to bring toughness and temperature performance.
Main Characteristics:
  • Free flow pellet
  • Medium Melt Flow Rate
  • Excellent compatibility with PP
  • Soft polypropylene<
Applications:
  • Blown film
  • Cast film
  • BOPE
  • BOPP
  • Sealant
Compiles with: US FDA 21 CFR 176.170©; US FDA FCN 909

Availability: Asia Pacific; Europe; Latin America; North America

Agency Ratings: FDA 21 CFR 176.170©; FDA FCN 909

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.891 g/ccISO 1183
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90Injection Molded; ASTM D2240
Tensile Strength at Break 4680 psiCompression Molded; ASTM D638
Elongation at Break 860 %Compression Molded; ASTM D638
Flexural Modulus 95600 psi1% Secant, Compression Molded; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 248 °F
Vicat Softening Point 225 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Gloss 60 %60°, Compression Molded; ASTM D523
 61 %20°, Compression Molded; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF580 / 311273

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.