MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
CRP Technology Windform® PS Polystyrene for Selective Laser Sintering  (discontinued **)
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Windform® PS is a polystyrene based material, developed specifically to produce complex investment casting patterns. The sintered patterns are ideal for conventional wax infiltration, and become easy to handle and finish. Windform® PS patterns are designed to work within regular rapid casting procedures, including autoclave and flash firing steps, low-temperature furnaces and vacuum plaster casting methods. Improved properties that make the difference, are: Improved surface quality and fine feature preservation; Reduced “curling” effect on the first layers; Very low ash content, therefore well suited for highly reactive alloys, such as Titanium, Aluminum, Magnesium, Steel and Nickel based alloys..

Sample applications: Complex investment casting patterns; Casting with highly reactive alloys, as well as conventional cast alloys. The casting structure is formed from an aggregate of grains or polyhedral crystallites which produce isotropic compensation: it is obvious that isotropy has great advantages, for instance, FEM calculations are very close to the real behaviour of the part.

Information provided by CRP Technology.

Vendors:   About CRP Technology
CRP Technology (Modena, Italy) develops, manufactures and sells its proprietary high performance composite materials Windform® for professional 3D Printing. It is also distinguished by its know-how in Selective Laser Sintering technology. It offers part production for short- and low-run production, and prototyping services with Windform®. Its specific application fields including but are not limited to: automotive and motorsports, design, aerospace, UAVs, marine, entertainment, defense, and packaging.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Bulk Density 0.380 - 0.480 g/ccTap; ASTM D4164
Moisture Absorption at Equilibrium <= 0.10 %ISO 62
Particle Size 52 µmLaser diffraction; d50; ISO 13320
 25 - 100 µmLaser diffraction; 90% range; ISO 13320
Ash <= 0.020 %ASTM D482
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 87.5 °CDSC

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CRP Technology Windform® LX 2.0 Polyamide Composite
CRP Technology Windform® GT Polyamide Glass Composite
CRP Technology Windform® XT 2.0 Polyamide-Carbon Fiber Composite
CRP Technology Windform® SP Polyamide-Carbon Fiber Composite for 3D Printing

PCRPT44 / 130420

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.