MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Unipetrol A+ High-Conductive Carbon Black Chezacarb
Categories: Carbon; Carbon Black

Material Notes: Carbon black Chezacarb is manufactured by gasification of heavy petroleum residues by partial oxidation in Shell reactors. It is produced in the form of pellets of size 0,5 - 2,5 mm. Product is not classified as dangerous according to EC Directives. Carbon black Chezacarb is made in three sorts: A+, A and B. There are suitable mostly for modification of conductance and heat conductivity in plastics and rubber, due to their high specific surface and high poresity.

Information provided by Unipetrol RPA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density >= 0.118 g/cc
 0.140 - 0.160 g/ccTamped Bulk Density
pH 7.0 - 9.0
Specific Surface Area 815 - 1005 m²/gby nitrogen absorption
Iodine Absorption Number 1010 - 1140mg/g
Ash <= 0.35 %
Evaporation Loss <= 0.30 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 40.0 ohm-cm
 
Component Elements PropertiesOriginal ValueComments
Iron, Fe <= 0.030 %
Nickel, Ni <= 0.050 %
Sulfur, S <= 0.23 %
Vanadium, V <= 0.10 %
 
Descriptive Properties
Compositionmax. 5
DBP Absorption (ml/100g)365-395
MaterialFines content
Pellets Hardness - average (g), max10
Pellets Hardness - the highest (g), max20
Toluene Extraction %, max0.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TIMCAL ENSACO™ 250G Conductive Carbon Black Compounds
92% Alumina, opaque
Basalt
Calcium Hydroxyapatite, Ca10(PO4)6(OH)2
Silicon Carbide, Alpha SiC

PUNIP116 / 82976

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.