System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Total Finathene® 5302 HDPE drain tile, corrugated pipe resin
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
;
High Density Polyethylene (HDPE), Pipe Grade
Material Notes:
Applications: corrugated pipe, storm and sanitary sewers, drainage systems
Information provided provided by Total Petrochemicals.
Total Petrochemicals includes former Fina and Atofina plastics product lines.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.953
g/cc
ASTM D 792
Environmental Stress Crack Resistance
40
hour
ASTM D1693 cond. B 100% lgepal
Melt Flow
0.35
g/10 min
@Load 2.16 kg
ASTM D 1238
High Load Melt Index
25
g/10 min
@Load 21.6 kg
ASTM D 1238
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
>=
3900
psi
ASTM D 638 type IV
Elongation at Break
>= 600 %
ASTM D 638 type IV
Flexural Modulus
190000
psi
ASTM D 790
Izod Impact, Notched
4.50
ft-lb/in
@Thickness 3.17 mm
ASTM D256
Thermal Properties
Original Value
Comments
Melting Point
263
°F
ASTM D3417
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Petromont 4101 High Density Polyethylene Resin
Petromont 4100 High Density Polyethylene Resin
Total Finathene® CD 522 HDPE corrugated pipe resin
Braskem BU004 Blow Molding High Density Polyethylene
Borealis BL2631 High Density Polyethylene
PFINAP114 / 38697
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.