MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Rigid Molding M3900 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.33 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cmASTM D955
Spiral Flow 88.9 cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75ASTM D2240
Tensile Strength, Yield 37.9 MPaType I, 51 mm/min; ASTM D638
Elongation at Break 60 %Type I, 51 mm/min; ASTM D638
Tensile Modulus 2280 MPaType I, 51 mm/min; ASTM D638
Flexural Strength 65.5 MPaASTM D790
Flexural Modulus 2280 MPaASTM D790
Izod Impact, Notched 210 J/m
@Thickness 3.18 mm,
Temperature -18.0 °C
Injection Molded; ASTM D256A
 590 J/m
@Thickness 3.18 mm,
Temperature 0.000 °C
Injection Molded; ASTM D256A
 750 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 71.1 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
 77.2 °C
@Thickness 6.35 mm
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
 72.8 °C
@Thickness 6.35 mm
Annealed; ASTM D648
UL RTI, Electrical 90.0 °CUL 746
UL RTI, Mechanical with Impact 85.0 °CUL 746
UL RTI, Mechanical without Impact 90.0 °CUL 746
Flammability, UL94 V-0
@Thickness 1.40 mm
ALL; UL 94
 V-0
@Thickness 1.50 mm
All Colors
 5VB
@Thickness 1.91 mm
All Colors
 5VB
@Thickness 1.40 mm
ALL; UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 199 - 210 °C
 
Descriptive Properties
FeaturesGeneral Purpose
 High Flow
 Low Temperature Impact Resistance
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAppliances
 Business Equipment
 Construction Applications
 Electrical/Electronic Applications
 General Purpose
 Telecommunications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Fittings M1012 Polyvinyl Chloride, Rigid
Colorite Polymers 2002 Rigid PVC
Axiall 9109J Clear Rigid PVC, Extrusion, Clear
Geon® Performance Solutions Vinyl Rigid Extrusion 87555 Polyvinyl Chloride, Rigid
Geon® Performance Solutions 80510 Polyvinyl Chloride, Rigid

PH0POL0148 / 144717

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.