MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Thermal Ceramics Kaowool Blanket
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Kaowool blanket is produced from kaolin, a naturally occurring alumina-silica fire clay. Kaowool, the world’s most recognizable name in ceramic fiber blanket, is available in a wide variety of densities and sizes. Kaowool blanket offers excellent handleability and high temperature stability. This allows it to meet a wide range of hot face and backup insulation applications in furnaces, kilns and other equipment requiring high temperature heat containment.

Military Specifications and Approvals:

  • Mil-I-23128A- 3, 6 pcf blanket
  • Mil-I-24244- all blankets
  • Mil-I-23128B- 6, 8 pcf blanket
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 0.0480 g/ccAvailable in multiple densities
     0.0640 g/ccAvailable in multiple densities
     0.0960 g/ccAvailable in multiple densities
     0.128 g/ccAvailable in multiple densities
     0.192 g/ccAvailable in multiple densities
    Thickness 3125 - 50000 microns
     
    Thermal PropertiesOriginal ValueComments
    Thermal Conductivity 0.0600 W/m-K
    @Temperature 260 °C
    8 pcf
     0.0700 W/m-K
    @Temperature 260 °C
    6 pcf
     0.0800 W/m-K
    @Temperature 260 °C
    4 pcf
     0.120 W/m-K
    @Temperature 538 °C
    8 pcf
     0.150 W/m-K
    @Temperature 538 °C
    6 pcf
     0.190 W/m-K
    @Temperature 538 °C
    4 pcf
     0.210 W/m-K
    @Temperature 816 °C
    8 pcf
     0.250 W/m-K
    @Temperature 816 °C
    6 pcf
     0.260 W/m-K
    @Temperature 982 °C
    8 pcf
     0.300 W/m-K
    @Temperature 1093 °C
    8 pcf
     0.320 W/m-K
    @Temperature 982 °C
    6 pcf
     0.330 W/m-K
    @Temperature 816 °C
    4 pcf
     0.430 W/m-K
    @Temperature 982 °C
    4 pcf
    Melting Point 3200 °F
    Maximum Service Temperature, Air 2000 °FContinuous
     2300 °FRating
     
    Component Elements PropertiesOriginal ValueComments
    Al2O3 45 %
    Alkalis 0.20 %
    B2O3 0.080 %
    CaO 0.10 %
    Fe2O3 1.0 %
    SiO2 50 - 55 %
    TiO2 1.7 %
     
    Descriptive Properties
    MgO Contenttrace
    Water Leachable Elements on Surface of Fiber, PPMBoron, 40
     Chlorine, <10
     Fluorine, <5
     Silicate, 125
     Sodium, 40
     Sulfur, 10

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Thermal Ceramics Kaowool Bulk Fiber
    Morgan Advanced Ceramics Ceramic Fiber Papers STD Paper Ceramic Fiber
    Morgan Advanced Ceramics Ceramic Fiber Papers AZS Paper Ceramic Fiber
    Morgan Advanced Ceramics Cerafelt Refractory Fiber Felt
    Morgan Advanced Ceramics Cerachrome™ Blanket Thermal Ceramic

    CTHERM000 / 2320

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.