MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Surlyn® 1650SB
Categories: Polymer; Film; Thermoplastic; Ethylene Methyl Acrylate

Material Notes: DuPont™ Surlyn® 1650SB is available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Slip and antiblock agents are added to reduce the film coefficient of friction and prevent film roll locking.

Applications:

  • Meat, poultry, seafood, and cheese packaging
  • Cereal liners
  • Medical/pharmaceutical packaging
  • Powdered/granular food and non-food pouches
  • Edible oil, motor oil, and other liquid product pouches
  • Snack structures
  • Coextrusions with nylon or in other film structures as a heat seal
  • Information provided by DuPont™

    This former DuPont product line is now a Dow product line.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Melt Flow 1.6 g/10 min
    @Load 2.16 kg,
    Temperature 190 °C
    ASTM D1238, ISO 1133
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength at Break 42.1 MPaTD; ASTM D882
     5105 psiMD; ASTM D882
    Elongation at Break 350 %MD; ASTM D882
     350 %TD; ASTM D882
    Impact 27J/mm, Spencer Impact; ASTM D3420
    Elmendorf Tear Strength, MD 13.9 g/micronASTM D1922
    Elmendorf Tear Strength, TD 15.1 g/micron
    Dart Drop 9.80 g/micronASTM D1709
    1% Secant Modulus, MD 37000 psiASTM D882
    1% Secant Modulus, TD 35000 psiASTM D882
     
    Thermal PropertiesOriginal ValueComments
    Melting Point 72.0 °CFreezing Point; ASTM D3418
     96.0 °CASTM D3417- ISO 3146
    Vicat Softening Point 73.0 °CASTM D1525, ISO 306
     
    Optical PropertiesOriginal ValueComments
    Haze 10.5 %ASTM D1003
    Gloss 20 %20°; ASTM D2457
     
    Processing PropertiesOriginal ValueComments
    Rear Barrel Temperature 149 °C
    Middle Barrel Temperature 191 °C
    Front Barrel Temperature 191 °C
    Die Temperature 375 °F

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Dow Surlyn® 8945 Thermoplastic Ionomer Resin
    Dow Surlyn® 2601 Sodium Ionomer Resin for Blown and Cast Film
    Dow Surlyn® 1601 Sodium Ionomer Resin for Blown and Cast Film
    Dow Surlyn® 9945 Thermoplastic Ionomer Resin
    Dow Surlyn® SG201U NC010 Supergloss Molding Alloy

    PDUP957 / 33524

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.