MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Trogamid® CX7323 Transparent Nylon  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon, Amorphous Transparent Alloy

Material Notes: Description: TROGAMID® CX compounds round off the product range of High Performance Polymers to include semicrystalline polyamides, the crystallites of which are so small that they do not scatter visible light—a property known as microcrystallinity. The compounds are therefore as clear as glass. They possess higher resistance to chemicals and stress cracking than amorphous transparent plastics, in addition to the mechanical advantages of amorphous compounds. The outstanding properties of TROGAMID® CX are:
  • crystal-clear, permanent transparency; high transmission
  • superior chemical and stress cracking resistance
  • high level of UV resistance
  • low water absorption, which leaves the mechanical properties virtually unaffected
  • high dimensional stability
  • balanced mechanical property profile
  • high impact resistance, even at low temperatures
  • high level of dynamic strength (e.g., for internally pressurized parts)
  • abrasion and scratch resistance
  • high glass transition temperature
  • very low isotropic shrinkage
  • easy processing

The unique combination of properties in TROGAMID® CX compounds permits their use over a broad application spectrum. Areas of application can be as diverse as water management, filter technology, laboratory and medical technology, the manufacture of eyeglasses, or bottles for the cosmetics industry.

Specific Notes for this Material: Medium-viscous, permanently transparent polyamide for injection molding and extrusion

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Key Words: PA PACM 12, cycloaliphatic diamine dodecanedioic acid
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
Melt Density 0.900 g/cc
@Temperature >=250 °C
Water Vapor Transmission 8.30 g/m²/day
@Diameter 0.108 mm,
Temperature 23.0 °C
85% R.H.
Oxygen Transmission Rate 37.49 cc/m²/day
@Diameter 0.0500 mm
or 740 cc/m²-24hr-bar
Nitrogen Transmission 4.31 cc-mm/m²-24hr-atm
@Diameter 0.0500 mm
or 85 cc/m²-24hr-bar
Carbon Dioxide Transmission 128.68 cc-mm/m²-24hr-atm
@Diameter 0.0500 mm
or 2540 cc/m²-24hr-bar
Viscosity Number 160 - 180 cm³/gISO 307
Permeability 5.0e-10cm3/(cm s bar), Nitrogen Permeation Coefficient (d=0.05 mm)
 4.3e-9cm3/(cm s bar), Oxygen Permeation Coefficient (d=0.05 mm)
 1.42e-8cm3/(cm s bar), Carbon Dioxide Permeation Coefficient (d=0.05 mm)
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 110 barBurst Pressure; Degussa
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 81ISO 868
Ball Indentation Hardness 108 MPaH30; ISO 2039-1
Tensile Strength at Break >= 50.0 MPa
@Temperature 23.0 - 80.0 °C
50 mm/min; ISO 527-1/2
Tensile Strength, Yield 60.0 MPa
@Temperature 23.0 - 80.0 °C
50 mm/min; ISO 527-1/2
Elongation at Break >= 150 %50 mm/min; ISO 527-1/2
 >= 50 %
@Temperature 80.0 °C
ISO 527-1/2
Elongation at Yield 9.0 %5 mm/min, Outer fiber strain at maximum stress; ISO 178
 8.0 %
@Temperature 23.0 - 80.0 °C
50 mm/min; ISO 527-1/2
Tensile Modulus 1.40 GPaISO 527-1/2
 1.27 GPa
@Temperature 80.0 °C
ISO 527-1/2
Flexural Strength 50.0 MPa5 mm/min, at 3.5% Strain; ISO 178
 90.0 MPa5 mm/min; ISO 178
Flexural Modulus 1.70 GPaISO 178
Charpy Impact Unnotched NB
@Temperature 0.000 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 1.40 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 1.50 J/cm²
@Temperature 0.000 °C
ISO 179/1eA
 1.60 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1 hour 1300 MPaISO 899-1
Tensile Creep Modulus, 1000 hours 700 MPaISO 899-1
Abrasion 18Abrasion Resistance, mg/100 rev.; DIN 53754
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+17 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohmIEC 60093
 >= 1.00e+15 ohmSpec.; IEC 60093
Dielectric Constant 3.2
@Frequency 1e+6 Hz
IEC 60250 DIN VDE 0303-Part 4
 3.6
@Frequency 100 Hz
IEC 60250 DIN VDE 0303-Part 4
Dielectric Strength 27.0 kV/mmK20/P50; IEC 60243-1
Dissipation Factor 0.0115
@Frequency 100 Hz
IEC 60250 DIN VDE 0303-Part 4
 0.0325
@Frequency 1e+6 Hz
IEC 60250 DIN VDE 0303-Part 4
Comparative Tracking Index 575 VTest Solution A, 100 drops; IEC 60112
 600 VTest Solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
Longitudinal; ISO 11359
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359
Specific Heat Capacity 2.49 J/g-°C
Thermal Conductivity 0.250 W/m-K
Melting Point 250 °C10 K/min
Maximum Service Temperature, Air 100 °CTemperature Index (Criterion: stress and yield); IEC 216
Deflection Temperature at 0.46 MPa (66 psi) 122 °CISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 105 °CISO 75-1/2
Vicat Softening Point 130 °C50N; ISO 306
 138 °C10N; ISO 306
Glass Transition Temp, Tg 140 °CTg, 10 K/min
Flammability, UL94 HB
@Thickness 0.800 mm
 HB
@Thickness 1.60 mm
Glow Wire Test 850 °C
@Thickness 1.00 mm
IEC 60695-2-1/0-3
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified
 
Descriptive Properties
Carreau-WLF K1559.3
Carreau-WLF K20.00187
Carreau-WLF K30.7486
Carreau-WLF K4300
Carreau-WLF K5176.3
ColorTransparent
Dynamical Behavior Under Load Min 106 cycles(Filter Cup/O-38 bar/160 min-1)
Scratch Resistance32% Turbidity IncreaseDIN 52347

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Trogamid® CX9701 Transparent Nylon
Evonik Trogamid® CX9710 Transparent Nylon
Evonik Trogamid® A4000 Transparent Polyamide
Evonik Trogamid® T5000 Nylon 6-3
EMS-Grivory Grilamid® TR 90 UV PAMACM12

PHUK118 / 47252

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.