MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lyanchemicals Tech SN321 Chloroprene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Chloroprene rubber is a polymer made from the monomer 2-chloro-1,3-butadiene. Neoprene is an important variety of synthetic rubber, not only has excellent light resistance, aging resistance, flexural resistance, acid and alkali resistance, oil resistance and heat resistance, but also has good physical and mechanical properties; its comprehensive performance is incomparable to other synthetic rubber. it is widely used in national defense, transportation, construction, light industry and military industry. Neoprene is mainly used in the production of automotive parts, machinery and industrial products and adhesives.

Main application: Mine conveyor belts, power transmission belts, hoses, seals, cushions, wire and cable jackets

Information provided by Lyanchemicals Tech Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 34 - 49
@Temperature 100 °C
ML(1+4)
 
Descriptive Properties
ModifierFour sulfide + Sulfur

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLYANT026 / 318053

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.