MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zoltek™ PX35 Pultruded Carbon Fiber/Epoxy Profile
Categories: Polymer; Thermoset; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Pultrusion is a cost-effective, continuous process for producing fiber-reinforced composite parts. ZOLTEK PX35 carbon fiber tows are fed into a proprietary impregnation and curing process which creates engineered carbon fiber profiles. These profiles enable rapid section buildup when laminating thick parts such as wind blade spar caps. High fiber alignment achieved with pultrusion delivers consistently superior properties in laminates compared to any other composite manufacturing processes.

APPLICATIONS: • Wind Energy (pre-cured carbon composite as the structural member of the turbine blade) • Infrastructure • Offshore Drilling • Mining

PERFORMANCE PROPERTIES: • High Stress & Stiffness • Corrosion Resistant • High Fiber Volume • Extremely Low Void Content • Locked In Filament Alignment.

Property data for a 6.4 mm diameter rod; fiber loading not reported but MatWeb estimates 62%.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 2200 MPa319000 psi
Elongation at Break 1.4 %1.4 %Epoxy
Tensile Modulus 150 GPa21800 ksi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zoltek™ PX35 Pultruded 62% Carbon Fiber/Epoxy Plate
PlastiComp Complet® LCF40 - PP Homopolymer Polypropylene, 40% Long Carbon Fiber Reinforced
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel
Goodfellow Carbon/Epoxy Composite Tube
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Strength 12k carbon UD tape supported S25 150 g/m2

PZOL844 / 232320

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.