MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Industeel FORA 400 Wear Resistant Steel, 400 HB
Categories: Metal; Ferrous Metal; Carbon Steel; Medium Carbon Steel

Material Notes: FORA 400 is a water quenched martensitic steel, with a typical hardness of 400HB (42.5 HRC), constituting a real answer to abrasive wear. Thanks to its toughness, its elevated hardness, its high yield strength, FORA 400 can be used wherever wear resistance to wear by sliding or by moderate impacts is required. Compared to conventional steels, such as S355, FORA 400 offers a real benefit to equipment life times and allows a significant thickness reduction in designs since its wear resistance is up to 3 times longer than S355 grade. Moreover, FORA 400 is very easily welded and has good forming properties thereby contributing to ease off fabrication. This steel is particularly suitable for applications in quarries, construction industry, mines, cement plants, iron and steel industry, etc.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 360 - 440Typical
Hardness, Rockwell C 39 - 47Typical
Tensile Strength, Ultimate 1350 MPaTypical
Tensile Strength, Yield 1100 MPaTypical
Elongation at Break 13 %Typical
Charpy Impact 35.0 J
@Temperature -20.0 °C
Typical
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.20 %
Chromium, Cr 1.0 %
Iron, Fe 96.875 - 96.9 %As remainder
Manganese, Mn 1.6 %
Molybdenum, Mo 0.30 %
Phosphorus, P <= 0.020 %
Sulfur, S <= 0.0050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ThyssenKrupp XABO® 355 Structural Steel
Industeel FORA 500 500 HB Wear Resistant Steel
ASTM A284 Steel, grade C
ThyssenKrupp PAS 355 Structural Steel for Cold Forming
The NanoSteel® Company SHS 9700 Steel Alloy, Wear Plate

NINDUST60 / 17598

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.