MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Bayhydrol® UV 2280 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Urethane acrylate dispersion. Bayhydrol® UV 2280 is used in the formulation of aqueous UV-curing coatings. Because of its very good initial physical drying, it is particularly suitable for use in aqueous pigmented UV-curing coatings.

Properties / Applications: Bayhydrol® UV 2280 is used in the formulation of aqueous UV-curing coatings, especially for application on wood/wood materials. Generally speaking, the coated surfaces can be sanded before UV curing. Additions of 1 - 2.5 % by wt. photoinitiator, calculated on the solid binder, have proved suitable for initiating the curing reaction. The viscosity is adjusted by the addition of polyurethane thickeners. If antifoams are used, they should be thinned in solvents, especially if application is by curtain coating. Matting agents and additives can be dispersed directly in the product using a dissolver. Bayhydrol® UV 2280 is easily matted using standard matting agents. As a rule, the coatings should be colored using aqueous pigment pastes. After evaporation of the water, the coatings can be cured at a belt speed of up to 10 m/min per 80 W/cm lamp. Ga-doped lamps and special photoinitiators are normally used in the curing of pigmented systems. To ensure optimum curing, it is important that the film contains no water and that thermal predrying has taken place. Depending on the formulation, the paint films are physically dry and sandable after evaporation of the water. However, they have no chemical or mechanical resistance. UV curing yields films with very good mechanical and chemical resistance. Bayhydrol® UV 2280 is also characterised by its good adhesion on many metallic substrates. Combination with Bayhydur® allows the formulation of aqueous dual-cure systems.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 60 - 62 %1g/1h/125 °C/convection oven; DIN EN ISO 3251
pH 6.8 - 8.2DIN ISO 976
 
Descriptive Properties
Appearancecolloidal
Flow time12-70s4 mm cup

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Blue River Coatings Hyfro-Flex Polyurethane Top Coat
Covestro Bayflex® WR-20 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Covestro Baytec® P-132 Polyurethane
Covestro Bayhydrol® A 2542 Polyurethane Coating
Covestro Bayhydrol® A 2470 Polyurethane Coating

PCOVEST0183 / 201966

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.