MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
RheTech Products P257-00 Polypropylene Copolymer, Natural
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Applications:
  • Splash shield and fender liners
  • Electrical enclosures
  • Underhood components

Injection molding conditions reported in table.

Information provided by RheTech Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/cc
@Temperature 23.0 °C
23/23°C; ASTM D792
Linear Mold Shrinkage 0.0145 cm/cmASTM D955
Melt Flow 16 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
Tensile Strength at Break 3000 psi2 in/min; ASTM D638
Flexural Modulus 140000 psiTangent; ASTM D790
Izod Impact, Notched 6.00 ft-lb/in
@Temperature 23.0 °C
ASTM D256
Gardner Impact 15.0 ft-lbASTM D5420
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 180 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 370 - 420 °F
Middle Barrel Temperature 380 - 430 °F
Front Barrel Temperature 390 - 440 °F
Nozzle Temperature 400 - 420 °F
Mold Temperature 80.0 - 120 °F
Drying Temperature 150 - 180 °F
Dry Time 1 - 2 hour
Moisture Content <= 0.050 %Recommended
Injection Pressure 400 - 1500 psi
Hold Pressure 300 - 1200 psi
Back Pressure 50.0 - 150 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RheTech Products FRP257-00 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Natural

PRHET301 / 65869

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.