MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LATI Lasulf PSU
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: Polysulfone (PSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/cc
Linear Mold Shrinkage, Flow 0.0060 - 0.0090 cm/cm
Linear Mold Shrinkage, Transverse 0.0065 - 0.0095 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break >= 100 %
@Temperature 23.0 °C
 >= 100 %
@Temperature 60.0 °C
 >= 100 %
@Temperature 90.0 °C
 >= 100 %
@Temperature 120 °C
 >= 100 %
@Temperature 150 °C
Elongation at Yield 2.8 %
@Temperature 150 °C
 3.5 %
@Temperature 120 °C
 4.0 %
@Temperature 90.0 °C
 4.5 %
@Temperature 60.0 °C
 5.5 %
@Temperature 23.0 °C
Tensile Modulus 1900 MPa
@Temperature 150 °C
 2000 MPa
@Temperature 120 °C
 2200 MPa
@Temperature 90.0 °C
 2300 MPa
@Temperature 60.0 °C
 2500 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched NB
@Temperature 23.0 °C
 NB
@Temperature -20.0 °C
Charpy Impact, Notched 1.50 kJ/m²
@Temperature -20.0 °C
 5.00 kJ/m²
@Temperature 23.0 °C
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 150 VA solution
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
Deflection Temperature at 0.46 MPa (66 psi) 180 °C
Deflection Temperature at 1.8 MPa (264 psi) 165 °C
Vicat Softening Point 175 °C
@Load 5.00 kg
Flammability, UL94 HB
@Thickness 1.50 mm
 V-1
@Thickness 3.00 mm
Oxygen Index 30 %
Glow Wire Test 960 °C
@Thickness 1.00 mm
GWFI/GWT
 960 °C
@Thickness 2.00 mm
GWFI/GWT
 
Processing PropertiesOriginal ValueComments
Melt Temperature 290 - 320 °C
Mold Temperature 110 - 130 °C
Drying Temperature 110 - 130 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Gharda Chemicals GAFONE™-S 1400 PSU, High Thermal Stability
Evonik Trogamid® CX7323 Transparent Nylon
BASF Ultrason® S 2010 PSU
Ensinger NORYL® Polyphenylene oxide (PPO)
LATI Lasulf G/30 PSU, 30% Glass Fiber Reinforced

PLATH9671 / 177367

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.