MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell DP 8220M Polybutene  (discontinued **)
Categories: Polymer; Thermoplastic; Polybutene

Material Notes:
Key Features: semi-crystalline, medium ethylene content random copolymer, reduces seal initiation temperature, FDA acceptable

Applications: seal-peel layer of BOPP film

Meets FDA requirements in 21 CFR 177.1570 for direct food contact up to 212°F (100°C).

Description: Polybutene-1 DP 8220 is a development product. It is a semi-crystallinel, medium ethylene content random copolymer which is miscible with polypropylenes due to its similar molecular structure. In blends with polyehtylenes it is immiscible but easily dispersible. The main target application for this experimental grade has been designed for use in blends with polypropylene, to reduce the seal initiation temperature. A typical application is the seal-peel layer of BOPP film formulations used for high speed packaging applications. By varying the concentrations of th blend components, seal initiation temperatures down to 75°C can be achieeived. This grade can be used in easy-opening applications where the optical properties of the peelable seal are critical. This resin meets FDA requirements for direct food contact at temperatures up to 100°C under regulation 21 CFR 177.1570.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.897 g/ccASTM D1505
Melt Flow 2.0 g/10 minISO 1133-1981E
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 26.0 MPaISO 1184-1983E
Tensile Strength, Yield 9.00 MPaISO 1184-1983E
Elongation at Break >= 350 %ISO 1184-1983E
Modulus of Elasticity 0.115 GPaISO 1184-1983E
 
Thermal PropertiesOriginal ValueComments
Melting Point 105 °CDSC
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
Overview of materials for Polybutene
LyondellBasell DP 8510M Polybutene
LyondellBasell DP 8310M Polybutene
Overview of materials for Nylon 6, Impact Grade

PMO711 / 53726

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.