MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

3D Systems Accura® Xtreme White 200 Plastic
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Ultra tough white plastic to replace CNC Machined polypropylene and ABS articles

    Features
  • Exceptionally tough and durable
  • Used for challenging functional assemblies
    • Used for snap fit assemblies
    • Used for master patterns for vacuum casting

    All information provided by 3D Systems.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density  1.12 g/cc
@Temperature 25.0 °C
0.0405 lb/in³
@Temperature 77.0 °F
Liquid
 1.18 g/cc
@Temperature 25.0 °C
0.0426 lb/in³
@Temperature 77.0 °F
Solid
Viscosity 650 - 750 cP
@Temperature 30.0 °C
650 - 750 cP
@Temperature 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 78 - 8078 - 80
Tensile Strength 45.0 - 50.0 MPa6530 - 7250 psiASTM D638
Elongation at Break 7 - 20 %7 - 20 %ASTM D638
Tensile Modulus 2.30 - 2.60 GPa334 - 377 ksiASTM D638
Flexural Strength 75.0 - 79.0 MPa10900 - 11500 psiASTM D790
Flexural Modulus 2.35 - 2.55 GPa341 - 370 ksiASTM D790
Izod Impact, Notched 0.550 - 0.600 J/cm1.03 - 1.12 ft-lb/inASTM D256
Penetration 4.64.6mils penetration depth
 
Thermal PropertiesMetricEnglishComments
CTE, linear  95.0 µm/m-°C
@Temperature 30.0 - 50.0 °C
52.8 µin/in-°F
@Temperature 86.0 - 122 °F
 180 µm/m-°C
@Temperature 70.0 - 140 °C
100 µin/in-°F
@Temperature 158 - 284 °F
Deflection Temperature at 0.46 MPa (66 psi) 47.0 °C117 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °C108 °FASTM D648
Glass Transition Temp, Tg 52.0 °C126 °FDMA, E"
 
Descriptive Properties
AppearanceWhite
Critical Exposure (mJ/cm²)8.3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
IRPC Polimaxx Porene SP100 Acrylonitrile Butadiene Styrene
3D Systems Accura® Xtreme Plastic for SLA® Systems
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography
Stratasys® Ultem 9085 for Rapid Prototyping
3D Systems RenShape® SL 7820 Stereolithography Plastic

PAPPR101g / 176024

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.