MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Formosa Plastics Formolene® E900 Pipe HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: High Density Polyethylene High Molecular Weight Bi-Modal Resin for Non-Pressure Pipe Extrusion Applications

Formolene® E900 is a high molecular weight high density polyethylene (HMW-HDPE) resin designed for non-pressure pipe applications. Formolene® E900 is well balanced in overall physical properties and provides good stiffness for extrusion applications.

Applications: Corrugated Pipe and Non-Pressure Pipe Extrusion Applications

Information provided by Formosa Plastics Corporation, USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.949 g/ccASTM D1505
Environmental Stress Crack Resistance 400 hour
@Strain 15 %
by NCLS; ASTM F2136
ESCR 10% Igepal® >= 500 hourCondition B; ASTM D1693
Melt Flow 0.040 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Condition E; ASTM D1238
High Load Melt Index 8.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
Condition F; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3600 psi2" (50mm) per min; ASTM D638
Elongation at Yield >= 600 %2" (50mm) per min; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -118 °CASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese GUR® 4120 PE-UHMW, Unfilled
Dow CONTINUUM™ DGDA-2490 NT Bimodal Polyethylene Resin
Chevron Phillips Marlex® HP076 High Density Polyethylene, Pipe Grade
Delrin Delrin® 500AF POM-SF20
Formosa Plastics Formolene® E924F Film HDPE

PFPCPQ056 / 150288

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.