MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Astralloy Astralloy-V® Alloy Steel Round Bars
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Astralloy-V round bars have the same chemistry, uniform toughness and hardness as plate, from surface to core. Astralloy-V’s ultra-fine grain structure, free of massive carbide particles due to its lower carbon content, provides better machinability at its higher strength/hardness level than quenched and tempered alloys.

Advantages:

  • Uniform hardness throughout the mass (340 BHN) to resist abrasion and promote slidability, and toughness to absorb impact without cracking.
  • Maintains its toughness and hardness without brittleness at temperatures of up to -75°F (-60°C).
  • Hardenability in the range of 550 BHN by impact or sliding action, without deformation or brittleness.
  • Astralloy-V’s small oxide surface quickly disappears, exposing a slick, durable surface.
  • Can be hot worked and allowed to air cool without loss of hardness or toughness and without warpage problems.

Information provided by Astralloy, a Nucor Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 320 - 388
Tensile Strength 175 ksi
Tensile Strength, Yield 153 ksi
Elongation at Break 15 %
@Thickness 50.8 mm
Charpy Impact 27.0 ft-lbLongitudinal
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -75.0 °F
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.29 %
Chromium, Cr <= 1.75 %
Iron, Fe >= 92.2 %As Balance
Manganese, Mn <= 1.05 %
Molybdenum, Mo <= 0.45 %
Nickel, Ni <= 3.9 %
Phosphorus, P <= 0.015 %
Silicon, Si <= 0.35 %
Sulfur, S <= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Stainless Steel
Astralloy 4330 V-Mod Alloy Steel Round Bars
Carlson 2205 (UNS S31803) Duplex Stainless Steel
Astralloy EB-450® Steel
Astralloy 4145 H-Mod Alloy Steel Round Bars

NNUCOR915 / 233189

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.