MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Polypropylene with 30% Talc Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Talc Filler

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.05 - 1.48 g/ccAverage value: 1.13 g/cc Grade Count:226
Filler Content 25.0 - 32.0 %Average value: 29.2 % Grade Count:81
Water Absorption 0.000 - 0.0500 %Average value: 0.0256 % Grade Count:16
Linear Mold Shrinkage 0.00500 - 0.0212 cm/cmAverage value: 0.0111 cm/cm Grade Count:133
Linear Mold Shrinkage, Transverse 0.00700 - 0.0211 cm/cmAverage value: 0.0125 cm/cm Grade Count:52
Melt Flow 0.500 - 230 g/10 minAverage value: 13.9 g/10 min Grade Count:212
Ash 25.0 - 32.0 %Average value: 29.8 % Grade Count:18
 28.0 - 30.0 %
@Temperature 700 - 900 °C
Average value: 29.0 % Grade Count:2
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 49.0 - 100Average value: 67.0 Grade Count:4
Hardness, Rockwell R 45.0 - 100Average value: 79.2 Grade Count:25
Hardness, Shore D 64.0 - 82.0Average value: 72.2 Grade Count:18
Ball Indentation Hardness 44.0 - 58.0 MPaAverage value: 51.7 MPa Grade Count:3
Tensile Strength, Ultimate 13.0 - 37.3 MPaAverage value: 26.0 MPa Grade Count:114
Tensile Strength, Yield 2.48 - 72.0 MPaAverage value: 25.3 MPa Grade Count:118
Elongation at Break 3.00 - 250 %Average value: 24.9 % Grade Count:113
 >= 100 %
@Temperature 60.0 - 90.0 °C
Average value: 100 % Grade Count:1
Elongation at Yield 2.70 - 80.0 %Average value: 7.90 % Grade Count:73
 5.00 - 6.00 %
@Temperature 60.0 - 90.0 °C
Average value: 5.50 % Grade Count:1
Modulus of Elasticity 1.50 - 4.00 GPaAverage value: 2.66 GPa Grade Count:55
 0.500 - 1.10 GPa
@Temperature 60.0 - 90.0 °C
Average value: 0.800 GPa Grade Count:1
Flexural Yield Strength 20.0 - 105 MPaAverage value: 46.2 MPa Grade Count:97
Flexural Modulus 1.40 - 19.7 GPaAverage value: 2.60 GPa Grade Count:224
 2.60 - 3.70 GPa
@Temperature -20.0 - -20.0 °C
Average value: 3.15 GPa Grade Count:2
Izod Impact, Notched 0.149 - 2.67 J/cmAverage value: 0.531 J/cm Grade Count:82
 0.300 - 1.00 J/cm
@Temperature -40.0 - 0.000 °C
Average value: 0.512 J/cm Grade Count:3
Izod Impact, Unnotched 0.470 - 5340 J/cmAverage value: 3.31 J/cm Grade Count:16
Izod Impact, Notched (ISO) 2.00 - 40.0 kJ/m²Average value: 10.2 kJ/m² Grade Count:53
 1.90 - 3.50 kJ/m²
@Temperature -40.0 - -30.0 °C
Average value: 2.62 kJ/m² Grade Count:13
Charpy Impact Unnotched 2.50 J/cm² - NBAverage value: 4.93 J/cm² Grade Count:58
 1.10 J/cm² - NB
@Temperature -40.0 - 0.000 °C
Average value: 2.64 J/cm² Grade Count:30
Charpy Impact, Notched 0.200 - 3.50 J/cm²Average value: 0.978 J/cm² Grade Count:98
 0.0300 - 0.600 J/cm²
@Temperature -40.0 - -20.0 °C
Average value: 0.277 J/cm² Grade Count:63
Gardner Impact 0.565 - 36.2 JAverage value: 5.23 J Grade Count:25
 5.53626 - 5.53626 J
@Temperature -30.0 - -30.0 °C
Average value: 6.89 J Grade Count:1
 7.23 - 7.23 J
@Temperature -23.0 - -23.0 °C
Average value: 6.89 J Grade Count:2
 7.23 - 7.23 J
@Thickness 3.18 - 3.18 mm
Average value: 6.89 J Grade Count:2
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+16 ohm-cmAverage value: 1.00e+16 ohm-cm Grade Count:3
Surface Resistance 1.00e+13 ohmAverage value: 1.00e+13 ohm Grade Count:5
Dielectric Constant 2.40 - 2.60Average value: 2.50 Grade Count:4
Dielectric Strength 19.7 - 24.0 kV/mmAverage value: 22.3 kV/mm Grade Count:5
Comparative Tracking Index 600 VAverage value: 600 V Grade Count:6
 
Thermal PropertiesOriginal ValueComments
CTE, linear 48.6 - 100 µm/m-°CAverage value: 75.2 µm/m-°C Grade Count:14
Melting Point 150 - 182 °CAverage value: 159 °C Grade Count:21
Deflection Temperature at 0.46 MPa (66 psi) 54.0 - 144 °CAverage value: 118 °C Grade Count:128
Deflection Temperature at 1.8 MPa (264 psi) 50.0 - 143 °CAverage value: 72.0 °C Grade Count:155
Vicat Softening Point 45.0 - 192 °CAverage value: 104 °C Grade Count:119
Flammability, UL94 HB - V-0Grade Count:89
Oxygen Index 21.0 %Average value: 21.0 % Grade Count:6
Glow Wire Test 550 - 750 °CAverage value: 726 °C Grade Count:33
 
Processing PropertiesOriginal ValueComments
Processing Temperature 193 - 227 °CAverage value: 210 °C Grade Count:3
Nozzle Temperature 200 - 260 °CAverage value: 222 °C Grade Count:20
Adapter Temperature 200 - 210 °CAverage value: 205 °C Grade Count:6
Die Temperature 200 - 210 °CAverage value: 205 °C Grade Count:6
Melt Temperature 170 - 279 °CAverage value: 219 °C Grade Count:99
Mold Temperature 10.0 - 90.0 °CAverage value: 48.6 °C Grade Count:94
Drying Temperature 51.7 - 220 °CAverage value: 80.2 °C Grade Count:81
Moisture Content 0.0500 - 0.200 %Average value: 0.0688 % Grade Count:20
Injection Pressure 2.76 - 130 MPaAverage value: 68.9 MPa Grade Count:63

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene with 20% Talc Filler
Overview of materials for Polypropylene with 40% Talc Filler
Overview of materials for Polypropylene with 10% Talc Filler
Overview of materials for Polypropylene with 30% Glass Fiber Filler
Overview of materials for Polypropylene, Molded

O4763 / 78400

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.