MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mearthane Durethane™ F DF-225A Closed Cell Foam Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: TDI backbone: ester.
Shore 00 Hardness: 70

Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient of friction, abrasion resistance, hardness and density) to suit various application. The rebound can be formulated for resiliency or energy absorption.

Applications: Applications for Durethane F include self-cleaning paper feed rollers, retard pads, conveyor belts, bumpers shock absorbers and timing belts.

Conductivity: All Durethane elastomers can be formulated to be electrically conductive, for applications involving electrostatic dissipation (ESD). Mearthane's proprietary conductivity process does not comprise the material performance specification of the urethane.

Information provided by Mearthane Products Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.640 g/cc0.0231 lb/in³ASTM D3574A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2525ASTM D2240
Tensile Strength, Ultimate 10.3 MPa1490 psiASTM D3574E
Elongation at Break 230 %230 %ASTM 3457E
100% Modulus 0.455 MPa
@Strain 100 %
66.0 psi
@Strain 100 %
Compressive Yield Strength 0.0700 MPa10.2 psiat 10% deflection; ASTM D3574C
 0.170 MPa24.7 psiat 20% deflection; ASTM D3574C
 0.260 MPa37.7 psiat 30% deflection; ASTM D3574C
Resilience 3434Bashore Rebound; ASTM 2632D
Tear Strength Test 4040lb; Die C; ASTM 3457F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mearthane Durethane™ F DF-640A Closed Cell Foam Polyurethane
Mearthane Durethane™ F DF-245A Closed Cell Foam Polyurethane
Mearthane Durethane™ F DF-620A Closed Cell Foam Polyurethane
Mearthane Durethane™ F DF-255A Closed Cell Foam Polyurethane
Covestro Bayfill® EA 2003 Polyurethane Energy-Absorbing Semi-Rigid Foam, Friable Grade, MDI-based 2-Component Liquid System

PMEA53 / 52548

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.