MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Silikony Polskie Polastosil M-99 Silicone Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: Rubber with strong hardness

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccBefore Curing
Viscosity 900 cPBefore Curing
Linear Mold Shrinkage 0.025 cm/cmAfter Curing
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65After Curing
Tensile Strength at Break 2.00 MPaAfter Curing
Elongation at Break 100 %After Curing
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °C
 
Processing PropertiesOriginal ValueComments
Cure Time <= 24.0 hourCuring
Pot Life 10 minCuring
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATG s.r.l. ACM Polyacrylic Rubber
Armacell Monarch® F-06905 (Gray) NBR/PVC Foam
Armacell Monarch® F-02003 (Black) Neoprene Based Rubber Foam
Silikony Polskie Polsil Gum 410/30 HTV Silicone Rubber
Silikony Polskie Polsil Gum 100/40 HTV Silicone Rubber

PPOLSI002 / 84302

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.