MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ganpati Exim BP93 Citric Acid Monohydrate
Categories: Other Engineering Material

Material Notes: Citric acid is a weak organic acid. It is a natural preservative and is also used to add an acidic, or sour, taste to foods and soft drinks. In biochemistry, it is important as an intermediate in the citric acid cycle and therefore occurs in the metabolism of almost all living things. It also serves as an environmentally benign cleaning agent and acts as an antioxidant. Citric acid exists in a variety of fruits and vegetables, most notably citrus fruits. Lemons and limes have particularly high concentrations of the acid; it can comprise as much as 8% of the dry weight of these fruits (1.44 and 1.38 grams per ounce of the juices, respectively).

Applications: Citric Acid is mainly used as acidulant, flavouring agent, preservative and antistaling agent infood and beverage industry. Moreover, it is also used as antioxidant, plasticizer and detergentin chemical, cosmetics and cleaning industries.
1. In the food industry, it is used as the acidulant in the making of soda, candy, biscuit, can,jam, juice and so on. Moreover, it can be used as the antioxidant of grease.
2. In the medicine industry, it is the raw material of many pharmaceuticals, such as ferricammonium citrate (blood tonic), sodium citrate (blood transfusion

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Ash <= 0.10 %Sulphated
 
Processing PropertiesOriginal ValueComments
Moisture Content 7.5 - 9.0 %
 
Descriptive Properties
AppearanceColorless Crystals or White Crystalline Powder
Content<1 ppmArsenic
 <10 ppmHeavy Metals (as Pb)
 <150 ppmSulphate
 <200 ppmCalcium
 <350 ppmOxalate
 <50 ppmChloride
 <50 ppmIron
 99.5-101%Content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGANPATI104 / 317388

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.