MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NuSil R-1130 Silicone One Part Sealing & Adhesive
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: General Purpose: One Part Sealing & Adhesive

Comments: Adhesive, Non-slump

Cure System: Oxime

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3535
Tensile Strength at Break 5.90 MPa856 psi
Elongation at Break 325 %325 %
Shear Strength 3.60 MPa522 psiLap
Tear Strength 7.01 kN/m40.0 pli
 
Processing PropertiesMetricEnglishComments
Cure Time 10100 min
@Temperature 25.0 °C
168 hour
@Temperature 77.0 °F
Tack-Free Time 25.0 min0.417 hour
 
Descriptive Properties
ColorTranslucent
Flow0.5 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NuSil MED-2213 Elastomeric Dispersion Biomedical Elastomer
LyondellBasell Lupolen 2420 K LDPE, Film Grade
LyondellBasell Lupolen 2420 H LDPE, Film Grade

PNUSIL010 / 141734

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.