System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Celanese Celanex® 3425HRT PBT, Glass Reinforced
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
Material Notes:
Celanex 3425HRT is a non-lubricated, 40% fiberglass reinforced PBT copolymer that has excellent hydrolysis resistance, toughness, improved flow, and improved elongation at break.
Information provided by Celanese
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.58
g/cc
ISO 1183
Moisture Absorption
0.120 %
23°C/50%RH; ISO 62
Linear Mold Shrinkage, Flow
0.00
-
0.0050
cm/cm
ISO 294-4
0.020
-
0.040
cm/cm
ASTM D955
Linear Mold Shrinkage, Transverse
0.0060
-
0.0090
cm/cm
ISO 294-4
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
107
MPa
5mm/min; ISO 527-2/1A
Elongation at Break
3.0 %
5mm/min; ISO 527-2/1A
Tensile Modulus
9100
MPa
50mm/min; ISO 527-2/1A
Flexural Strength
165
MPa
ISO 178
Flexural Modulus
8500
MPa
ISO 178
Izod Impact, Notched (ISO)
11.0
kJ/m²
ISO 180/1A
Charpy Impact Unnotched
53.0
kJ/m²
ISO 179/1eU
44.0
kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched
11.0
kJ/m²
ISO 179/1eA
9.40
kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+16
ohm-cm
IEC 60093
Surface Resistance
3.00e+17
ohm
IEC 60093
Dielectric Constant
4.13
@Frequency 1e+6 Hz
IEC 60250
4.21
@Frequency 100 Hz
IEC 60250
Dielectric Strength
31.0
kV/mm
IEC 60243-1
Dissipation Factor
0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
375
V
IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
20.0
µm/m-°C
ISO 11359-2
CTE, linear, Transverse to Flow
116
µm/m-°C
ISO 11359-2
Melting Point
225
°C
10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi)
202
°C
ISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi)
175
°C
ISO 75-1, -2
Glass Transition Temp, Tg
20.0
°C
ISO 11357-1,-2,-3
Processing Properties
Original Value
Comments
Processing Temperature
65.0
-
93.0
°C
cavity
250
-
260
°C
hot runner
Feed Temperature
230
-
240
°C
Zone 1
230
-
240
°C
Zone 2
235
-
250
°C
Zone 3
235
-
250
°C
Zone 4
240
-
260
°C
Die Temperature
250
-
260
°C
Melt Temperature
235
-
260
°C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Celanese Celanex® 3202-2 PBT, Glass Reinforced
Celanese Celanex® 3226 PBT, Glass Reinforced
Celanese Celanex® 3209HR PBT, Glass Reinforced
Celanese Thermx® TE1001 BK010 PCT
Celanese Thermx® CG943 NC010T PCT
PHCQ062 / 178517
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.