MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Go Yen Chemical Electric Welding Rod TiO2 Titanium Dioxide
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Advantages:
  • isolating air
  • protecting melted metal
  • preventing air entrance
  • Deoxidizing
  • denitrifying
  • reforming mechanical property
  • Adding alloy element
  • Stabilized
  • Propitious to vertical-position welding
  • Arcing fast
  • Little Impurity contentontent
  • produce cold seam
  • Granule is small and average, sieved remaining of 45µm sieve pore should be less 0.5%
Applications:
  • welding rod
  • Slag-making agent, with excellent deoxidization effect
  • well welding thinner, adhesive, arc stabilizer
  • applied on alternating current
  • direct current welding rods
  • reduce SO2 consumption during produced process, making surface smooth, make arc easily
  • Other application of specific industry products.

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.90 g/cc0.141 lb/in³
Oil Absorption 24.0 %24.0 %
Particle Size 45 µm45 µm0.1% Residue
pH 6.5 - 8.06.5 - 8.0Water Suspension
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.50 %<= 0.50 %
 
Component Elements PropertiesMetricEnglishComments
TiO2 >= 98.5 %>= 98.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN544 / 266852

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.