MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik TEGO® AddBond 1270 Adhesion resin solution
Categories: Other Engineering Material

Material Notes: Special features:
  • for solvent borne formulations
  • after neutralization with amines suitable for waterborne formulations
  • good adhesion improvement on metal
  • improves the corrosion protection
Application:
  • industrial coatings recommended addition level solid calculated on binder solid: 3.0 - 15.0 %

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 30 %
Viscosity 6500 cP
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 60[mg KOH/g], calculated on non-volatile content
 
Descriptive Properties
Hydroxyl Number10 mg KOH/gcalculated on non-volatile content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik TEGO® AddBond LTH Solid adhesion resin
Evonik TEGO® AddBond 2325 Adhesion resin solution
Evonik TEGO® AddBond 2220 ND Adhesion resin solution
Evonik TEGO® AddBond HS Adhesion resin solution
Evonik TEGO® AddBond LTW Adhesion resin solution

PEVONIL664 / 196868

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.