System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
LG Chemical KEYFLEX BT 5035D Ester Type TPE
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Polyester, TP
;
Polyester Thermoplastic Elastomer
Material Notes:
Description: Injection Molding, TPC-ET, Specialty, Low Modulus, Black Color
Application: Automotive Body Plug, Fastener
CAS: 37282-12-5 and 1333-86-4
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.11
g/cc
1.11
g/cc
ASTM D792
Water Absorption
0.60 %
@Temperature 23.0 °C,
Time 86400 sec
0.60 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Maximum Moisture Content
0.010
0.010
Injection Molding
Linear Mold Shrinkage, Flow
0.010
-
0.014
cm/cm
@Thickness 3.20 mm
0.010
-
0.014
in/in
@Thickness 0.126 in
ASTM D955
Melt Flow
30
g/10 min
@Load 2.16 kg,
Temperature 230 °C
30
g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
88
88
ASTM D2240
Hardness, Shore D
35
35
ASTM D2240
Tensile Strength at Break
24.5
MPa
@Thickness 2.00 mm
3550
psi
@Thickness 0.0787 in
50mm/min; ASTM D638
Elongation at Break
700 %
@Thickness 2.00 mm
700 %
@Thickness 0.0787 in
50mm/min; ASTM D638
Flexural Modulus
0.0490
GPa
@Thickness 6.40 mm
7.11
ksi
@Thickness 0.252 in
15mm/min; ASTM D790
Izod Impact, Notched
NB
@Thickness 6.40 mm,
Temperature 23.0 °C
NB
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
NB
@Thickness 6.40 mm,
Temperature -40.0 °C
NB
@Thickness 0.252 in,
Temperature -40.0 °F
ASTM D256
Electrical Properties
Metric
English
Comments
Comparative Tracking Index
600
V
600
V
Solution A; IEC 60112
Thermal Properties
Metric
English
Comments
Melting Point
200
°C
392
°F
Peak
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
200
-
220
°C
392
-
428
°F
Injection Molding
Middle Barrel Temperature
205
-
225
°C
401
-
437
°F
Injection Molding
Front Barrel Temperature
210
-
230
°C
410
-
446
°F
Injection Molding
Nozzle Temperature
210
-
230
°C
410
-
446
°F
Injection Molding
Melt Temperature
200
-
230
°C
392
-
446
°F
Injection Molding
Mold Temperature
10.0
-
35.0
°C
50.0
-
95.0
°F
Injection Molding
Drying Temperature
80.0
-
90.0
°C
176
-
194
°F
Injection Molding
Dry Time
3.00
-
4.00
hour
3.00
-
4.00
hour
Injection Molding
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
LG Chemical KEYFLEX BT 3028D Ester Type TPE
LG Chemical KEYFLEX BT 1030D Ester Type TPE
LG Chemical KEYFLEX BT 3038D Ester Type TPE
LG Chemical KEYFLEX BT 3140D Ester Type TPE
LG Chemical KEYFLEX BT 2140D Ester Type TPE
PLAY441 / 148451
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.