MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 FR Fluid-Glycol ISO Grade 32
Categories: Fluid; Lubricant

Material Notes: FR Fluid-Glycol is a water-glycol based fire-resistant hydraulic fluid developed for use in industrial hydraulic systems operating in areas subject to fire hazards. It contains sufficient water to snuff out a fire resulting from ignition of a fluid leak. It is suitable for use in hydraulic systems operating at 2,000 to 3,000 psi, and can withstand intermittent pressure spikes up to 5,000 psi. FR Fluid-Glycol is formulated with diethylene glycol, 40% water and select additives that provide lubricity, wear protection and corrosion protection. It has good antiwear properties to ensure long life for hydraulic pumps and motors. Special rust and corrosion inhibitors provide corrosion protection in both the liquid phase and the vapor phase. The high water content provides fire resistance if the fluid comes into contact with an ignition source. This product contains less than 60 parts per billion (ppb) phenols, and does not contain any nitrites or nitrosamines. It is compatible with other water-glycol type fire-resistant hydraulic fluids. FR Fluid-Glycol is compatible with most hydraulic pumps, including vane, piston and gear pumps. It is safe to use with most packing and seal materials except polyurethane and silicone. Cork shaft seals should be replaced with Buna N or other synthetic rubber. Leather packing should be avoided and zinc or cadmium-plated components should not be used.

Applications: Hydraulic systems on equipment operating in areas subject to fire hazards, such as in:

  • Steel and aluminum mills
  • Molding and metal die casting machinery
  • Welding machines
  • Foundries
  • Furnace charging equipment
  • Open hearth and basic oxygen furnace (B.O.F.) equipment
  • Power transmission plants
FR Fluid-Glycol meets the requirements of the following OEM specifications:
  • Denison Hydraulics HF-4
  • U.S. Steel 171
Features/Benefits:
  • Fire-resistant for safety
  • Excellent wear protection for hydraulic pumps and motors
  • Excellent rust and corrosion protection
  • Good foam resistance
  • Glycol content protects against freezing
  • Compatible with other water-glycol fluids

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/cc
Density 1.08 g/cc0.0390 lb/in³
pH 9.79.7neat
Viscosity Measurement 202202Index
Saybolt Viscosity at 100°F 198 SUS198 SUS
Saybolt Viscosity at 210°F 54.7 SUS54.7 SUS
Kinematic Viscosity at 40°C (104°F) 39.3 cSt39.3 cSt
Kinematic Viscosity at 100°C (212°F) 8.5 cSt8.5 cSt
 
Mechanical PropertiesMetricEnglishComments
Four Ball Wear 0.480 mm0.0189 inScar Diameter; ASTM D4172
 
Thermal PropertiesMetricEnglishComments
Melting Point -55.0 °C-67.0 °FFreezing Point
 
Processing PropertiesMetricEnglishComments
Moisture Content 40 %40 %
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5056 / 198309

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.