MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Unreinforced

Material Notes: By special additives, impact strength and abrasion resistance are further improved. Manufacturer recommends this material for slipper pads for rolling mills.

Color: Ivory

Applications: slipper pads for rolling mills.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccDry Density
Moisture Absorption at Equilibrium 2.5 - 3.0 %50% RH
Water Absorption at Saturation 6.0 - 7.0 %23°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 76 - 78DIN 53505
Tensile Strength at Break 63.0 - 65.0 MPaDIN 53455
Elongation at Break 100 - 150 %DIN 53455
Tensile Modulus 2.00 GPaDIN 53457
 0.300 GPa
@Temperature 100 °C
DIN 53457
Charpy Impact, Notched 6.00 - 12.0 J/cm²DIN 53453
Coefficient of Friction 0.050 - 0.10to steel, added lubrication
 0.30 - 0.35to steel, no lubrication; ISO/DTR 7147
Tensile Creep Modulus, 1000 hours <= 450 MPaDIN 53444
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+12 - 5.00e+12 ohm-cmDIN 53482
Surface Resistance 1.00e+10 - 3.00e+10 ohmDIN 53482
Dielectric Constant 12
@Frequency 1e+6 Hz
DIN 53483
Dielectric Strength 15.0 - 20.0 kV/mmDIN 53481
Dissipation Factor 0.15
@Frequency 1e+6 Hz
DIN 53483
Comparative Tracking Index 600 VKV Method; DIN 53480
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 1.67 J/g-°C
Thermal Conductivity 0.280 W/m-KDIN 52612
Melting Point 205 °C
Maximum Service Temperature, Air 100 - 120 °Clong time operation
 120 - 140 °Cmedium time operation
 160 °Ca few hours operation
Minimum Service Temperature, Air -40.0 °C
Flammability, UL94 HB
 
Descriptive Properties
Permissible Unit Pressure25 - 30 MPa
Time yield limitup to 8s1/1000; DIN.53444

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ashley Polymers Ashlene® 982 Nylon 612
Zell-Metall Engineering Plastics Zellamid 1115
Domo TECHNYL® eXten D 458P PA6.10, Conditioned
CHT Group QSil 7750 Addition Cure, Thermally Conductive Material
Chemours Teflon® PTFE Grade K-10 Fluoropolymer Resin

PZELL17 / 72946

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.