MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals Surpass® RMs244-U Octene sHDPE Rotational Molding Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Rotational Molding Grade

Material Notes:

Features:

  • Octene copolymer
  • Exceptional low temperature properties
  • Outstanding stiffness
  • Broad processing window
  • Superior whiteness for improved part appearance
  • Easy mold release
  • NSF listed for Standards 14, 24 and 61
  • Applications:

  • Custom Industrial parts
  • Storage tanks
  • Marine products
  • Materials handling containers
  • Information provided by Nova Chemicals

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 0.944 g/ccCompression Molded; ASTM D792
    ESCR 10% Igepal® 200 hourCompression Molded; ARM Method
    Melt Flow 1.7 g/10 min
    @Load 2.16 kg,
    Temperature 190 °C
    Compression Molded; ASTM D1238
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength, Yield 23.4 MPaCompression Molded; ASTM D638
     3410 psiRotational Molded; ASTM D882
    Flexural Modulus 0.950 GPaRotational Molded; ASTM D790
     0.980 GPaCompression Molded; ASTM D790
    Impact Test 217 J
    @Thickness 6.35 mm
    Compression Molded; ARM Method
     
    Thermal PropertiesOriginal ValueComments
    Melting Point 129.4 °CCompression Molded; ASTM E794
    Deflection Temperature at 0.46 MPa (66 psi) 66.0 °CCompression Molded; ASTM D648
    Deflection Temperature at 1.8 MPa (264 psi) 44.0 °CCompression Molded; ASTM D648

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    NOVA Chemicals SURPASS® RMs245-U sHDPE Rotational Molding Resin
    ICO Polymers ICORENE™ 150-1498 HDPE Rotational Molding Resin
    ICO Polymers ICORENE™ 150-1049 HDPE Rotational Molding Resin
    A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene
    NOVA Chemicals Surpass® RMs244-UG Octene sHDPE Rotational Molding Film

    PNOV932 / 54878

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.