MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayhydrol® A 2470 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Bayhydrol A 2470 is an aqueous hydroxyfunctional polyacrylic dispersion. Waterborne two-component polyurethane varnishes in combination with aliphatic polyisocyanates.

Properties / Applications: Bayhydrol A 2470 is a hydroxyfunctional polyacrylic dispersion which can be thinned with water to application viscosity. The viscosity of the product is largely governed by the pH. As the pH may decrease during storage, a decrease in viscosity is also to be expected. The viscosity can be restored to its original value by the addition of small amounts of an aqueous 10% solution of dimethyl ethanol amine. Bayhydrol A 2470 combined with aliphatic polyisocyanates yields high-gloss top coats which can be dried at room temperature or force-dried, e.g. at 80°C. The cured paint films are hard and flexible with outstanding resistance to solvents and water and excellent weatherability. Application of a clearcoat based on Bayhydrol A 2470 directly on wood may lead to discoloration. When properly formulated, e.g. in combination with Bayhydur 304 in an NCO / OH ratio of 1.5 : 1, the pot life is approximately 4 hours. Bayhydrol A 2470 has good pigment wetting properties and high shear stability. Bead mills have proved suitable as grinding equipment. Only pigments and extenders with a minimum water-soluble content should be used. Given the many pigments and extenders available, compatibility testing should always be carried out. When mixing Bayhydur or Desmodur into the mill base, a thickener must be added to ensure a high shear effect. The addition of approximately 0.4% Borchigen® PW 25 (calculated on the solid binder) has proved suitable for formulations based on Bayhydrol A 2470. Levelling and substrate wetting can be optimised by adding, for example Byk® 380. Byk® 011 has proved to be a suitable antifoam. Application and formulation equipment can be cleaned with water, alkaline cleaning agents or isopropanol. As with any product, use of Bayhydrol A 2470 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/cc
Volatiles 53 - 56 %53 - 56 %1g/1h/125 °C/convection oven
pH 7.0 - 8.07.0 - 8.01:4 in demineralized water
Viscosity 1500 - 3000 cP1500 - 3000 cPD= approx. 40 s-1
 
Chemical PropertiesMetricEnglishComments
Acid Value 1010[mg KOH/g]
 
Descriptive Properties
Content3.9%Hydroxyl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Acclaim® 2200 Polyol
Blue River Coatings Hyfro-Flex Polyurethane Top Coat
Covestro Bayflex® WR-20 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Covestro Baytec® P-132 Polyurethane
Covestro Desmodur® BL 1100/1 Polyurethane

PCOVEST0153 / 201936

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.