MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik SIPERNAT® D 10 Ceramic Powder
Categories: Other Engineering Material

Material Notes: SIPERNAT represents a specific product range of precipitated silica, aluminum and calcium silicates. SIPERNAT D 10 is a milled, hydrophobic (i.e. not wettable by water) silica with high methanol wettability. SIPERNAT D 10 is used in a great variety of defoamer due to its high effectiveness and ease of dispersion.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0800 g/cc0.00289 lb/in³Tamped; ISO 787-11
Particle Size 6.5 µm6.5 µmd50; ISO 13320-1
pH 10.310.35% in water; ISO 787-9
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) <= 8.0 %
@Temperature 1000 °C,
Time 7200 sec
<= 8.0 %
@Temperature 1830 °F,
Time 2.00 hour
ISO 3262-1
SiO2 >= 95 %>= 95 %ISO 3262-19
Sodium, Na <= 1.2 %<= 1.2 %
 
Descriptive Properties
Content<1.0%Sulfate
 <400 ppmIron

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik BREAK-THRU® AF 9908 Surfactants
Evonik SIPERNAT® 383 DS Silica Powder
Evonik SIPERNAT® 35 Silica Powder
Evonik SIPERNAT® 320 DS Silica Powder
Evonik SIPERNAT® 160 Ceramic Powder

PEVONIM074 / 197278

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.