MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CLAL-MSX NICLAL 1800 H14 4/4 Hard Copper Alloy, Free Cutting Nickel-Silver
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Main Characteristics:
  • Good corrosion resistance
  • High mechanical properties
Typical Applications:
  • Parts subject to high stress
  • High quality fasteners

Information provided by CLAL-MSX

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.75 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers >= 18
Tensile Strength, Ultimate 650 - 850 MPa
Tensile Strength, Yield >= 600 MPa
@Strain 0.2 %
Elongation at Break 3.0 %100 A
Modulus of Elasticity 130 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000260 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 0.000 - 100 °C
Specific Heat Capacity 0.420 J/g-°C
Thermal Conductivity 30.0 W/m-K
Melting Point 1060 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 62 %
Lead, Pb <= 1.0 %
Nickel, Ni 18 %
Zinc, Zn <= 19 %
 
Descriptive Properties
ColorSilvery

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Navy "M" Bronze, UNS C92200, Copper Casting Alloy
High Leaded naval brass, UNS C48500, H02 (20%) Temper rod
Copper, Cu; Cold Drawn
CLAL-MSX NICLAL 3444 H12 1/2 Hard Copper Alloy, Free Cutting Bronze
CLAL-MSX CUPROROR® TL4 Hard, Copper Alloy

NCLAL088 / 160119

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.