MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polycasa Acryl® KR 2010/1 Acrylic, Impact Grade
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Impact Modified, Molded

Material Notes: High-impact grade with good flowability (e.g. for lamp covers).

Data was collected by ISO methods.

Quinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/cc
Moisture Absorption at Equilibrium 0.40 %
Linear Mold Shrinkage, Flow 0.0065 cm/cm
Melt Flow 3.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 50.0 MPa
Elongation at Break 22 %
Elongation at Yield 5.0 %
Tensile Modulus 2.05 GPa
Charpy Impact Unnotched 7.00 J/cm²
Charpy Impact, Notched 0.500 J/cm²
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+14 ohm-cm
Surface Resistance 1.00e+14 ohm
Dielectric Constant 2.9
@Frequency 1e+6 Hz
 3.2
@Frequency 100 Hz
Dielectric Strength 60.0 kV/mm
Dissipation Factor 0.030
@Frequency 1e+6 Hz
 0.040
@Frequency 100 Hz
Comparative Tracking Index 600 V
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 110 µm/m-°C
@Temperature 20.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C
Vicat Softening Point 97.0 °C
Flammability, UL94 HB
@Thickness 1.60 mm
Oxygen Index 18 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polycasa Acryl® KR 2014/1 Acrylic, Impact Grade
Polycasa Acryl® KR 2015/1 Acrylic, Impact Grade
Kolon SPESIN® KP513 PBT Alloy Resin
Kolon SPESIN® KP270 General Purpose PBT Base Resin
Kolon SPESIN® KP213G15BL Glass Fiber Reinforced PBT Compound Resin

PSF021 / 66579

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.