MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Tetrashield™ MP2000 Polyester  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Product Description: Eastman Tetrashield™ MP2000 for metal packaging enhances the performance of Bisphenol A non-intent (BPA-NI) metal packaging coatings. With high solids, improved retort resistance, and broad chemical resistance, formulations featuring Tetrashield™ protective resin systems can achieve superior performance results in interior food contact metal packaging applications. Eastman Tetrashield™ MP2000 resin can also be used in ends, caps and closures, and general line applications to improve coating performance in these demanding applications as well as to formulate high solids coating formulations.

Application/Uses:

  • Coatings – Interior and exterior metal packaging - food
  • Coatings – Interior and exterior metal packaging - general
  • Interior caps and closures - food
Key Attributes:
  • Chemical resistance
  • Hardness
  • Reduced VOC
  • Retort/blush resistance

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 45 %
Viscosity 400 cP
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 3.0[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Boiling Point 254 °C@ 760 mm Hg
Glass Transition Temp, Tg 76.0 °C
 
Descriptive Properties
ColorAPHA
Hydroxyl Number15[mg KOH/g]

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Milliken® Millad® HBPA Hydrogenated Bisphenol A
Eastman Tritan™ MP100 Copolyester
Eastman Tritan™ FX200 Copolyester

PEATM5182 / 222376

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.