MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lucobit Lucosol® Bitumen Road Binder
Categories: Fluid; Solvent

Material Notes: Lucosol is a solvent based bitumen road binder made out of selected bitumen qualities and hydrocarbon solvents

Information provided by Lucobit AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 - 0.950 g/ccDIN 52004
Solids Content 70 - 80 %bitumen content by weight
Viscosity 2960 cP
@Temperature 40.0 °C
D-viscosity
Viscosity Measurement 90 - 110s; STV 4mm/40°C
 
Thermal PropertiesOriginal ValueComments
Flash Point 25.0 °CPensky-Martens
 100 °CD-flash point; DIN 51758
Ring & Ball Softening Point 60.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 70.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucobit Lucobit® 1220 Ethylene Copolymer Bitumen

PLUCO962 / 151028

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.