MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Hostaform® C 27021 XAP2® LS POM, UV Resistant
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Description: Easy flow injection molding grade with reduced emissions especially for automotive interior applications. With improved UV resistance.

Burning rate according to FMVSS 302 < 100 mm/min (1 mm thickness)

Emissions according to VDA 275 < 5 mg/kg

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccISO 1183
Water Absorption 0.65 %ISO 62
Melt Flow 24 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 64.0 MPa50 mm/min; ISO 527-2/1A
Elongation at Break 17 %50 mm/min; ISO 527-2/1A
Elongation at Yield 7.5 %50 mm/min; ISO 527-2/1A
Tensile Modulus 2.75 GPaISO 527-2/1A
Flexural Modulus 2600 MPaISO 178
Charpy Impact Unnotched 120 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 120 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 5.50 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 5.50 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1 hour 2400 MPaISO 899-1
Tensile Creep Modulus, 1000 hours 1200 MPaISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Constant 4.0
@Frequency 100 Hz
IEC 60250
 4.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 35.0 kV/mmIEC 60243-1
Dissipation Factor 0.0020
@Frequency 100 Hz
IEC 60250
 0.0050
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 1.10 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 1.10 µm/m-°CISO 11359-2
Melting Point 164 °C10°C/min; ISO 11357-1,-2,-3
 
Processing PropertiesOriginal ValueComments
Feed Temperature 60.0 - 80.0 °C
Nozzle Temperature 190 - 200 °C
Zone 1 170 - 175 °C
Zone 2 180 - 185 °C
Zone 3 180 - 195 °C
Zone 4 180 - 200 °C
Melt Temperature 180 - 200 °C
Mold Temperature 80.0 - 120 °C
Drying Temperature 120 - 140 °C
Dry Time 3 - 4 hour
Moisture Content <= 0.15 %
Injection Pressure 60.0 - 120 MPa
Hold Pressure 60.0 - 120 MPa
Back Pressure 0.000 - 4.00 MPa
Screw Speed 70 rpm
@Diameter 55.0 mm
 100 rpm
@Diameter 40.0 mm
 150 rpm
@Diameter 25.0 mm
 
Descriptive Properties
Hopper20-30°C
Manifold190-200°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hostaform® C 27021 AS POM, Specialty
Celanese Hostaform® C 27021 POM, Unfilled
Celanese Hostaform® C 27021 XAP² ™ POM, Unfilled
Celanese Hostaform® C 27021 TF POM, Tribological
Celanese Hostaform® C 27021 LS colored POM, UV Resistant

PHCX510 / 135135

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.