MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bohler-Uddeholm BeCu Alloy 172 Mold Material
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Beryllium copper alloy

A high strength beryllium copper mold alloy with high thermal conductivity.

BeCu Alloy 172 is characterized by:

  • High thermal conductivity
  • Good corrosion resistance
  • Good polishability
  • Good wear resistance
  • Good resistance to galling
  • Good machinability
  • High strength and hardness
  • Excellent weldability

The special properties of BeCu Alloy 172 beryllium copper alloy make it a suitable mold/core/insert material for a wide variety of molding situations but especially where a combination of high thermal conductivity, corrosion resistance and good polishability are needed.

  • Blow molds: pinch offs, neck rings and handle inserts.
  • Injection mold: molds, cores, inserts.
  • Injection nozzles and manifolds for hot runner systems.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.302 lb/in³
 0.297 lb/in³
@Temperature 299 °C
 0.299 lb/in³
@Temperature 199 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 30 - 40Age-hardened
Tensile Strength, Ultimate 170000 psihardened to 30 HRC
 185000 psihardened to 40 HRC
Tensile Strength, Yield 143500 psi
@Strain 0.2 %
hardened to 30 HRC
 157200 psi
@Strain 0.2 %
hardened to 40 HRC
Elongation at Break 6.0 %hardened to 40 HRC
 8.0 %hardened to 30 HRC
Modulus of Elasticity 19000 ksi
 15000 ksi
@Temperature 299 °C
 19000 ksi
@Temperature 199 °C
Compressive Yield Strength 970 MPa0.2%, hardened to 30 HRC
 1070 MPa0.2%, hardened to 40 HRC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.70 µin/in-°F
@Temperature 199 °C
 9.90 µin/in-°F
@Temperature 299 °C
Specific Heat Capacity 0.0910 BTU/lb-°F
@Temperature 20.0 °C
 0.114 BTU/lb-°F
@Temperature 199 °C
 0.128 BTU/lb-°F
@Temperature 299 °C
Thermal Conductivity 110 W/m-K
@Temperature 20.0 °C
hardened to 40 HRC
 120 W/m-K
@Temperature 20.0 °C
hardened to 30 HRC
 145 W/m-K
@Temperature 199 °C
hardened to 40 HRC
 155 W/m-K
@Temperature 299 °C
hardened to 40 HRC
 160 W/m-K
@Temperature 199 °C
hardened to 30 HRC
 170 W/m-K
@Temperature 299 °C
hardened to 30 HRC
 
Component Elements PropertiesOriginal ValueComments
Beryllium, Be 1.9 %
Co + Ni 0.25 %
Copper, Cu 97.85 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
IBC Advanced Alloys C17510 Beryllium Copper Alloy Plate, Temper A(TB00)
Aluminum Alloys, General
P & P Technology BeCu alloy 25 (CA172) Contact Finger Strips
Cadi MOLD-MOR™ 3
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy)

NBUCOR34 / 15503

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.