MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Indium Corp. Indalloy® 4 Pure Indium Solder
Categories: Metal; Nonferrous Metal; Indium Alloy; Solder/Braze Alloy; Pure Element

Material Notes: Soft, ductile metal has good wettability on many surfaces including ceramics, glass and quartz. Deforms indefinitely under load and has no tendency to become brittle, making it valuable for cryogenic applications.

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.31 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 0.90
Tensile Strength, Ultimate 1.90 MPa
Elongation at Break 22 - 41 %
Modulus of Elasticity 1570 ksi
Shear Strength 6.10 MPaShear Bond Holding Strength
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000720 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 28.47 J/g
CTE, linear 29.0 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.243 J/g-°CSolid
Thermal Conductivity 86.0 W/m-K
@Temperature 85.0 °C
Melting Point 157 °C
Solidus 157 °C
Liquidus 157 °C
 
Component Elements PropertiesOriginal ValueComments
Indium, In 100 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Indium, In
Indium Corp. 6N High Purity Indium Metal
Indium Corp. Indalloy 157 Lead Solder Alloy
Indium Corp. Indalloy® 117 Bi-Pb-In-Sn-Cd Fusible Alloy
Indium Corp. Indalloy® 290 In-Ag Solder Alloy

NNIN18 / 18474

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.