MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese SO.F.TER Forprene® 6NM.D50 TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Injection Molding, standard grade

Forprene is a Vulcanized Thermoplastic Elastomer. Applications include automotive (air ducts, pipe grommets, weather seals, glass encapsulation, belt line seals, air vents, buttons, mats, suspension bellows), building (extruded seals for doors and windows, simple or co-molded hydraulic seals), household appliances (anti-vibration mounts, inlet pipes and exhaust manifolds, seals, drum suspension bushes, shock absorbers), Tools (handles and grips), Electrical equipment (sheaths for condensers, plugs and loose sockets, special cables requiring good electrical insulation properties, UV-resistance, good thermal resistance and low specific gravity), and Miscellaneous (wheels, drive belts, high/low pressure pipes, mats for motor scooters, O-rings).

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D 792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 51ASTM D 2240
Tensile Strength 20.8 MPaASTM D412 C
Elongation at Break 650 %ASTM D412-C
100% Modulus 0.0122 GPa
@Strain 100 %
ASTM D412 C
Tear Strength 85.0 kN/mASTM D624 C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese SO.F.TER Forprene® 6NM.A35 TPE
Celanese SO.F.TER Forprene® 6NM.A40 TPE
Celanese SO.F.TER Laprene® 830.540 SEBS TPE
Celanese SO.F.TER Laprene® 830.541 TPE
Celanese SO.F.TER Laprene® 830.542 TPE

PSOFS681 / 162145

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.