MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Borlink™ LE0595-07 Polyethylene Compound, Crosslinkable, Semiconductive
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: LE0595-07 is a crosslinkable black polyethylene compound, specially designed for bonded semi conductive screen applications. LE0595-07 is a crosslinkable black polyethylene compound, specially designed for bonded semi conductive screen applications. Applications LE0595-07 is intended for semi conductive applications in XLPE medium and high voltage cables. It is developed for constructions with bonded insulation shields. Specifications: AEIC CS7; AEIC CS8; BS 6622; DIN VDE 0276-263; DIN VDE 0276-620; HD 620 S1; HD 632 S1; IEC 60502; IEC 60840; ISO 1872-E/BA, KHXY, 23-G200, C40; ICEA S-93-639; NF C33-223; NF C33-226; UTE C 33-223; and UL 1072.

Information provided by Borealis AG

Key Words: PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.135 g/ccASTM D1928C/D 792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 9.30 MPaafter aging (168h, 150°C)
 18.6 MPaASTM D638
Elongation at Break 200 %25mm/min; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 100 ohm-cm
@Temperature 90.0 °C
ASTM D991
 
Processing PropertiesOriginal ValueComments
Shelf Life 18.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Borlink™ LE0315 Polyethylene Compound, Crosslinkable, Semiconductive
Borealis LE0151 Easy Strippable Semiconductive Insulation Shield for Medium Voltage Power Cables
Borealis Borlink™ LE0310-44 Polyethylene Compound, Crosslinkable, Semiconductive
Borealis Superclean™ LR4201S Crosslinkable Polyethylene Insulation for Medium and High Voltage Power Cables
Borealis Borlink™ LE0592 Polyethylene

PBOREA513 / 108772

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.