MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Thermal Ceramics Smoothset (wet, air setting) Mortar
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Thermal Ceramics refractory mortars were developed to match Thermal Ceramics dense and insulating firebricks in various thermal, chemical and physical service conditions. Available in wet and dry grades, Thermal Ceramics mortars will provide the convenience you want with the performance you need for practically every high temperature refractory application. K-Bond Mortar has an extra smooth, creamy consistency plus excellent tackiness to brick surfaces.

Features:

  • Matched for use with each Thermal Ceramics firebrick and insulating firebrick
  • Both heat setting and air setting grades are available
  • Temperature use limits range from 2850°F to 3200°F
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Thermal PropertiesOriginal ValueComments
    Maximum Service Temperature, Air 2850 °F
     
    Processing PropertiesOriginal ValueComments
    Shelf Life 4.00 Month
     
    Component Elements PropertiesOriginal ValueComments
    Al2O3 36 %
    Alkalis 4.0 %
    CaO 0.20 %
    Fe2O3 0.90 %
    MgO 0.10 %
    SiO2 57 %
    TiO2 1.7 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
    Huntsman HY 1341 Cycloaliphatic Amine
    Chosun Refractories SP-60W High-Adhesion Mortar
    Chosun Refractories RAPN Special Mortar
    Chosun Refractories HSM-36 Heat-Setting Mortar

    CTHERM234 / 2554

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.