MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay RHODATERGE® BCC Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Rhodaterge® BCC is Surfactant Base for Low Foaming, Highly Alkaline Cleaners (45% solids). Delivers exceptional surface tension reduction in high caustic systems; stable in 50% Sodium Hydroxide. Rhodaterge® BCC is soluble and stable in 25% HCL and is very effective acidic cleaner applications. Low foaming, defoams protenaceous soils. It is also well suited for high pressure applications due to it's free rinsing nature and high tolerance of electrolytes. It is NSF registered cleaner.

Chemical Name: SURFACTANT BLEND

Available in: Asia Pacific, Europe, Latin America and North America

Applications: RHODATERGE® BCC is widely sold into the food tank cleaning industry and used extensively in brewery line cleaning operations due to its superior stability, low foaming properties, protein de-foaming capability and detergency in up to 50% sodium hydroxide and/or 45% potassium hydroxide. RHODATERGE® BCC is also well suited for high pressure applications due to its free rinsing nature and high tolerance for electrolytes. RHODATERGE® BCC is soluble and stable in 25% HCL and is very effective in acidic cleaner applications.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 - 1.11 g/ccRP-0549
Solids Content 40 - 45 %Moisture Balance; RP-0536
pH 7.510% Solution
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 200 °CClosed Cup
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceClean, Clear Amber LiquidRP-0064

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay RHODATERGE® MULTIGREEN II Surfactant
Solvay ANTAROX® B 12 DF Surfactant
Solvay IGEPAL® CO 210 Surfactant
Solvay MIRATAINE® ASC Surfactant
Solvay RHEOZAN SH Biopolymer

WRHOD459 / 137690

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.