MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Tenite 285A2R30018 Cellulose Acetate Butyrate, Natural, Trsp
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Cellulosic; Cellulose Acetate Butyrate, Molded

Material Notes: Applications:
  • Ophthalmics
  • Optical safety frames

Product Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. Tenite cellulose plastics are available in natural, clear, selected ambers, or smoke transparents and black translucents. Color concentrates are available in let-down ratios from 10:1 to 40:1. Tenite Cellulose Acetate Butyrate 285-18 has a plasticizer level of 18% and contains an odor mask.

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccASTM D792
Water Absorption 1.3 %
@Time 86400 sec
Immersion; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 26ASTM D785
Tensile Strength at Break 30.7 MPaASTM D638
Tensile Strength, Yield 23.5 MPaASTM D638
Elongation at Break 50 %ASTM D638
Flexural Strength 30.4 MPaASTM D790
Flexural Modulus 1034 MPaASTM D790
Izod Impact, Notched 110 J/m
@Temperature -40.0 °C
ASTM D256
 358 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 61.0 °CASTM D648
Vicat Softening Point 94.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified
 
Descriptive Properties
Formula Number285Odor Mask
Plasticizer18 percent
Soluble Matter Loss0.1 percentASTM D570
Weight Loss on Heating0.9 percentASTM D707, 72 hrs, 80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Cellulose Acetate Butyrate, Molded
Braskem JE 6190 Compression Molding Polypropylene
Rotuba H5 Cellulose Acetate
Celanese Acetate Tow
Eastman Tenite 307E4000018 Propionate Clear, Trsp

PE8825 / 129670

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.