MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Elastollan® B 60 A ESD TPUR
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and superior low temperature flexibility.

Typical Applications: Sport-shoe soles and accessories, ski-boot shells, technical moldings, e.g. seals, castor tyres and tubing.

Note: Quoted results are from measurements on injection molded test platens, post tempered for 20 hours at 100°C

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ISO 1183-1-A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565ISO 868
Tensile Strength 20.0 MPa2900 psiISO 37
 20.0 MPa2900 psiafter storage in water at 80°C for 42 days; ISO 37
Tensile Stress at Strain  1.00 MPa
@Strain 20 %
145 psi
@Strain 20 %
ISO 37
 2.50 MPa
@Strain 100 %
363 psi
@Strain 100 %
ISO 37
 6.50 MPa
@Strain 300 %
943 psi
@Strain 300 %
ISO 37
Elongation at Break 800 %800 %ISO 37
 900 %900 %after storage in water at 80°C for 42 days; ISO 37
Charpy Impact, Notched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DIN EN ISO 179
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DIN EN ISO 179
Tear Strength 40.0 kN/m228 pliDIN ISO 34-1/Bb
Abrasion 120120[mm3; ISO 4649
Compression Set  20 %
@Temperature 23.0 °C
20 %
@Temperature 73.4 °F
ISO 815
 30 %
@Temperature 70.0 °C
30 %
@Temperature 158 °F
ISO 815
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 230 °C347 - 446 °FInjection molding
Mold Temperature 20.0 - 70.0 °C68.0 - 158 °F
 
Descriptive Properties
Commercial StatusNorth America
Primary Processing TechniqueInjection molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Elastollan® 1175A10W Wire & Cable Grade Polyurethane Elastomer
BASF Elastollan® C 59 D TPUR
BASF Elastollan® S 50 A SPF TPUR
BASF Elastollan® R 2001 20% Glass Filled TPUR
Huntsman AVALON® 60 AE-ESD Thermoplastic Polyurethane

PBASG0497 / 132130

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.